Factors affecting precision casting accuracy

Time:2025-04-07 /Hot:0

In general, the dimensional accuracy of precision castings is influenced by various factors such as casting structure, casting material, mold making, shell making, roasting, pouring, etc. Any unreasonable setting or operation of any link can cause changes in the shrinkage rate of the casting, resulting in deviations from the required dimensional accuracy of the casting. The following are factors that can cause dimensional accuracy defects in precision castings:

(1) The influence of casting structure: a. Casting wall thickness, high shrinkage rate, casting wall thickness, low shrinkage rate. b. The free shrinkage rate is high, while the obstructed shrinkage rate is low.

(2) The influence of casting material: a. The higher the carbon content in the material, the smaller the linear shrinkage rate, and the lower the carbon content, the larger the linear shrinkage rate. b. The casting shrinkage rate of common materials is as follows: casting shrinkage rate K=(LM-LJ)/LJ × 100%, LM is the cavity size, and LJ is the casting size. K is influenced by the following factors: wax mold K1, casting structure K2, alloy type K3, and pouring temperature K4.

(3) The influence of mold making on the shrinkage rate of castings: a. The wax injection temperature, wax injection pressure, and holding time have a significant impact on the size of the investment mold, with wax injection temperature being the most important factor, followed by wax injection pressure. Holding time has little effect on the final size of the investment mold after ensuring its formation. b. The linear shrinkage rate of wax (mold) material is about 0.9-1.1%. c. When the investment mold is stored, further shrinkage will occur, with a shrinkage value of about 10% of the total shrinkage. However, after 12 hours of storage, the size of the investment mold is basically stable. d. The radial shrinkage rate of wax molds is only 30-40% of the longitudinal shrinkage rate, and the effect of wax injection temperature on the free shrinkage rate is much greater than that on the hindered shrinkage rate (the optimal wax injection temperature is 57-59 ℃, and the higher the temperature, the greater the shrinkage).

(4) The influence of shell making materials: The use of zircon sand, zircon powder, Shangdian sand, and Shangdian powder can be ignored due to their small expansion coefficient of only 4.6 × 10-6/℃.

(5) The influence of shell roasting: Due to the small expansion coefficient of the shell, when the shell temperature is 1150 ℃, it is only 0.053%, so it can also be ignored.

(6) The influence of casting temperature: The higher the casting temperature, the greater the shrinkage rate, and the lower the casting temperature, the smaller the shrinkage rate. Therefore, the casting temperature should be appropriate.


Edit:DeChang


?
主站蜘蛛池模板: 国产精品av免费观看 | 久久99中文字幕伊人 | 精品视频一区二区三三区四区 | 国产黄A片三級三級三級 | 影音先锋资源av不撸 | 国产亚洲欧美在线观看三区 | 国产亚洲欧洲日韩在线观看 | 一级人做人a爰免费视频 | 100国产精品人妻无码 | 亚洲AV高清一区二区三区色欲 | 小妖精朕受不了了高h | 91尤物在线| 色综合久久久久久888 | 日本网站在线播放 | 亚洲国产精品不卡毛片a在线 | 天上人间av网 | 国产白丝精品爽爽久久久久久蜜臀 | 综合亚洲桃色第一影院 | 秋霞网在线伦理免费 | 欧美日韩免费播放一区二区 | 国产一区免费在线观看 | 欧美一区二区三区大片 | 中文字幕欧美在线 | 91精品全国免费观看青青 | 日韩免费高清大片在线 | 最新在线黄色网址 | 99久久免费精品 | 国产视频精品久久 | 狠狠人妻久久久久久综合九色 | 欧美一区二区VA毛片视频 | 成人伊人网 | 国产亚洲自拍一区 | 丁香六月 | 中文字幕熟女人妻伦伦在线 | 狠狠色噜噜狠狠狠狠色综合网 | 欧美一区二区三区在线视频 | 亚洲A片成人无码久久精品色欲 | 一区二区三区无码被窝影院 | 91资源在线播放 | 天美传媒AV成人片免费看 | 向日葵APP网页进入 消息称老熟妇乱视频一区二区 |